Abstract
This paper presents the first effort to determine the elastic modulus ( E) and hardness ( H) of muscovite and rectorite by nanoindentation. Samples were examined under varying maximum load, loading rate, and hold time at the maximum load conditions. The measured E and H values were affected by: (1) numerous giant steps observed in the load–displacement curves, particularly under large loads; (2) maximum load; (3) loading rate; and (4) the hold time at maximum load. The two minerals behaved differently under indentation, owing to the difference in their crystal structure. Rectorite exhibited more highly time-dependent response and had much lower E and H values than muscovite. After correction by removing the giant steps to obtain more accurate E and H values, the dependence of E and H on the maximum load tended to disappear. The corrected values for E, 79.3 ±6.9 and 18.3 ± 4.6 GPa, and H, 5.14 ± 0.82 and 0.73 ± 0.17 GPa, for muscovite and rectorite, respectively, were in good agreement with the data published in the literature. This study also demonstrated the importance of choosing appropriate test control parameters in obtaining more reliable E and H values of layered aluminosilicates using nanoindentation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.