Abstract

The adiabatic elastic moduli of single crystals of lead containing 1%–17% thallium have been measured using the ultrasonic pulse echo technique. Data at room temperature, 77°, and 4.2°K were obtained. It was observed that increasing the thallium content decreased all the moduli in spite of the fact that the interatomic distance decreases with thallium additions. Values of the Debye θ0 parameter were calculated from the 4.2°K modulus values.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.