Abstract
The present paper accounts for the synthesis, crystal structure, differential scanning calorimetry and vibrational spectroscopy of a new compound (1,3,5-triazinidium-2,4,6-triamine) hexabromidodicuprate (II) grown at room temperature by slow evaporation of aqueous solution. From X-ray diffraction data collected at room temperature, it is concluded that it crystallizes in the monoclinic system (P21/c space group). The anion and the cation are linked by N–H···Br hydrogen bonds. Furthermore, the room temperature IR and Raman spectra of the title compound were recorded and analyzed. The differential scanning calorimetric has also been investigated. Hirshfeld surfaces were used to confirm the existence of inter-molecular interactions in the compound.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.