Removing acid from sulfuric acid alkylation reaction products through fiber media is a new and challenging process in the industry. In this paper, a filler braided from stainless-steel fiber and polytetrafluoroethylene fiber is used to separate the acid-hydrocarbon emulsion. The selected filler characteristics (fiber diameter is 50 μm, bed porosity is 58.3%) and operation condition (superficial velocity is 37.5 m/h) based on lab-scale experiments were applied in the industrial tests, and a good acid-hydrocarbon separation performance was obtained. The separation efficiency was 99.82% and the pressure drop was 43.4 kPa at the superficial velocity of 37.5 m/h. In addition, through the study of fiber wettability, the coalescence mechanism was revealed, which is that the special braided structure induces acid droplets and hydrocarbon droplets to move in different directions, and the droplets on the fiber continue to migrate, coalesce and grow up, thereby achieving the rapid separation of acid and hydrocarbon phases. These findings can facilitate further applications of the sulfuric acid alkylation technology and significantly improve environmental benefits.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.