Abstract

The reserve of the copper-oxide-bearing limonite ore (COBL ore) in Yulong Copper Co., Ltd. is up to 20 million tons with 1.79% of copper content. The characters of the copper resources in the COBL ore are high-proportioned oxidation state (99.98%) and combined state (84.83%). The combined copper oxide is mainly copper-oxide-bearing limonite, which has a copper content of more than 78%. Because of the high altitude and average annual temperature of 15 °C in Tibet, fire leaching cannot be adopted. The leaching efficiency of copper from COBL ore using direct leaching of sulfuric acid is only 40%, which is greatly influenced by temperature and time. Based on the characteristics of COBL ore, a novel combined method of magnetic separation and individual leaching has been proposed to efficient recover copper resources. Experimental results show that the magnetic concentrates and tailings were obtained by magnetic separation of COBL ore at 0.6 T with the yields were 59.65% and 40.35%, respectively. Due to the obvious leaching properties difference of the magnetic concentrates and tailings, individual leaching process routes were used to treat them. The magnetic concentrate was leached with stirring for 3 days at room temperature (20 °C), and the magnetic tailing was easily leached for 4 h at 40 °C. The recovery efficiency of total copper was 72%, which was about 32% higher than that of the single leaching of the COBL ore. The method proposed in this study achieves environmentally friendly, low energy consumption, and efficient extraction of refractory copper oxide ore.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call