Abstract

This work proposed a promising biorefinery method for the deconstruction of moso bamboo by using p-toluenesulfonic acid (P-TsOH) pretreatment to product high-purity cellulose (dissolving pulp). The cellulose pulp with high α-cellulose content (82.36 %) was successfully prepared for 60 min at low pretreatment temperature (90 °C) and atmospheric pressure. After the simple bleaching and cold caustic extraction (CCE) processes, the properties of cellulose pulp, such as α-cellulose content, polymerization, ISO brightness, all met the standard of dissolving pulp. In general, the cooking method through P-TsOH pretreatment can shorten the preparation time, which can effectively reduce energy consumption and chemical consumption. Therefore, this work may provide a new perspective for the green preparation of dissolving pulp that can be used to produce lyocell fiber after ash and metal ion treatment.