Developing an appropriate method to broaden the color of long persistent luminescence materials has important scientific significance and practical value but remains a great challenge. Herein, we have developed a unique strategy to fine-tune the persistent luminescence using the inclusion complex of rhodamine 6G with (2-hydroxypropyl)-β-cyclodextrin as efficient light conversion materials. The emitting color of the novel persistent luminescence material could be tuned from green to orange by changing the concentration of the light conversion agent. Furthermore, afterglow decay measurements showed that the initial afterglow brightness is 9.65 cd/m2, and the initial afterglow brightness gradually decreased as the cyclodextrin inclusion compound coating increased. This design concept introduces a new perspective for broadening the luminescence color of afterglow phosphors, which may open up new opportunities for persistent luminescence materials toward many emerging applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call