Abstract

Fe9Cr, Fe17Cr and Fe25Cr alloys were subjected to isothermal oxidation in Ar/O 2 and Ar/H 2 atmosphere at 700 °C as high temperature corrosion for 48 h. Oxidation weight change measurement showed increasing Cr content reduced the oxidation rate. The oxidized Cr alloys were analysed using SEM, TEM and XRD. The addition of water vapour accelerates the onset of breakaway oxidation kinetics for Fe9Cr. The presence of water vapour promotes internal oxidation of Cr within Fe9Cr. For Fe17Cr and Fe25Cr, the water vapour effect is not significant due to the large Cr reservoir due to continue growth of Cr 2O 3.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.