Abstract

Polymer alloys of benzoxazine resin (BA-a) and urethane prepolymer (PU) were prepared at various BA-a : PU mass ratios (100 : 0, 80 : 20, 70 : 30 and 60 : 40) via sequential cure method. Isocyanate end capped urethane prepolymer was synthesized with isocyanates and polyols. Various types of isocyanate groups were used [i.e., TDI, MDI, IPDI and HDI] in this study. Polypropylene glycol and Poly(ethylene, diethylene adipate) glycol represent polyether polyol (E) and polyester polyol (S), respectively. Experimental results revealed that glass transition temperature (Tg), flexural strength and flexural modulus increase with decreasing PU content. Furthermore, the flexural strength and flexural modulus synergism were found in the BA-a:PU based polyester polyol at all mass ratio.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.