Abstract
The effects of the γ″-Ni3Nb phase on the mechanical properties of Inconel 718 superalloys, with standard heat treatment, hot isostatic pressing + solution treatment + aging, and hot isostatic pressing + direct aging, were characterized by morphological observation, X-ray diffraction, and tensile experiments. The results of the morphological observation revealed that many fine γ″ precipitates of ~26.49 ± 1.82 nm in mean size were formed in all samples. However, the relatively coarser γ″ precipitates formed in the grain boundaries were only observed in the sample treated with hot isostatic pressing + direct aging. The yield strengths of the hot isostatic pressing + direct aging sample at room temperature and at 650 °C both exhibited the maximum values about 993 ± 5.7 and 811 ± 12.6 MPa, respectively. The γ″ precipitate was considered to be the dominant strengthening phase in the sample according to the lattice misfits (ε) of γ/γ″. The strengthening mechanism of the samples can be explained as the coherency strain strengthening of fine γ″ precipitates. Moreover, due to the coarser γ″ precipitates in the grain boundaries, dislocation-cut ordered particle strengthening also occurred in the sample after hot isostatic pressing + direct aging treatment.
Highlights
Inconel 718 superalloys have been used for a wide range of applications because of their excellent qualities such as good comprehensive mechanical properties, easy processing, relatively low cost, and outstanding weldability [1,2,3,4,5,6]
The effects of the γ” phase on mechanical properties of Inconel 718 superalloys with treatments of
standard heat treatment (SHT), hot isostatic pressing (HIP) + STA, and HIP + direct aging (DA) were investigated in this study
Summary
Inconel 718 superalloys have been used for a wide range of applications because of their excellent qualities such as good comprehensive mechanical properties, easy processing, relatively low cost, and outstanding weldability [1,2,3,4,5,6]. The related solidification defects, such as microporosity, dendritic segregation, and the formation of Laves and δ phases, have harmful effects on the mechanical properties of the cast superalloy [10]. To address this problem, hot isostatic pressing is required to close pores, homogenize the microstructure, and improve the mechanical properties of the cast Inconel 718 superalloy. In recent years, increasing attention has been focused on the hot isostatic pressing (HIP) of the Inconel 718 alloy which has a fine uniform microstructure and good mechanical properties [11,12,13,14]
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.