the hot extruded AZ31 magnesium alloy which has basal texture was impacted along different direction and different fracture mode appeared. Under different impacted direction, the basal slip, prismatic slip, pyramidal slip, compression twin and tension twin have different critical resolved shearing stress (CRSS) and Schmid factor. Then different deformation modes were activated and resulted to different fracture modes.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.