Abstract

The impact tensile properties of laser welded butt joints of two kinds of high strength steel plates with the tensile strength level of 590 MPa and 780 MPa (denoted by HR590 and HR780, respectively), were investigated using split Hopkinson bar tensile testing apparatus. Impact tension tests for the joint specimens pre-fatigued were also carried out to examine the effect of pre-fatigue. There were no significant effects of strain-rate and pre-fatigue on the dynamic and quasi-static tensile strength of laser welded butt joints. However, the decrease in the elongation of HR780 welded joints subjected high cycle pre-fatigue was observed only at a high strain-rate. From the observation of fracture surface, it was found that the decrease in the elongation may be caused by a number of damages due to the combination of high cycle pre-fatigue and high strain-rate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.