Abstract

The effect of steel slag substitution as coarse aggregate on compressive strength in fly ash based-geopolymer concrete was studied. The compressive strength was evaluated by measuring the maximum acceptable load using compression testing equipment. Compressive strength depends on several factors, such as time and temperature of curing and the mixing proportion. The compressive strength of geopolymer concrete with steel slag substitution was higher compared to geopolymer concrete with gravel aggregate. The optimum compressive strength was found on the third day of curing at a temperature of 60 o C for both the geopolymer concrete with steel slag substitution and normal geopolymer concrete. Reinforcement corrosion was evaluated by measuring the corrosion current density using a linear polarization potentiostatic scan. The corrosion rate of reinforcing steel in geopolymer concrete with steel slag substitution was found to be higher compared to normal geopolymer concrete without steel slag in seawater medium, whereas in an acid rain environment, steel slag substitution increased corrosion resistance. The corrosion rate of geopolymer concrete with steel slag substitution was found to be lower compared to normal geopolymer concrete. The corrosion rate was found to be very high at an early stage and decreased with time.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.