Abstract

Abstract Calcined spray-dried hydroxyapatite (Ca10(PO4)(OH)6; i.e., HA) powders were atmospherically plasma sprayed (APS) using various process parameters. The resulting phases within the coating surface and the interface between the coating and the substrate were analyzed using X-ray diffraction (XRD) methods. This XRD revealed the presence of both amorphous (i.e., amorphous calcium phosphate: ACP) and crystalline phases. The crystalline phases included both HA and some impurity phases from the decomposition of HA, such as tricalcium phosphate (α-TCP and β-TCP), tetracalcium phosphate (TTCP) and calcium oxide (CaO). The crystallinity of HA decreased with increasing spray power and stand-off distance (SOD). The percentage of all impurity phases increased with the spray power. The percentage of both TCP and TTCP decreased with the SOD while the CaO percentage increased. In addition, the percentage of ACP and CaO were higher in the interface than at the surface of the coating while the percentage of TCP and TTCP exhibited the opposite effect.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.