Abstract

Three layer clad brazing sheets composed of Al-7.5Si alloy (filler, thickness:10 ㎛ )/Al-1.2Mn-2Zn-(0.04-1.05)Si alloy (core, thickness:80 ㎛)/Al-7.5Si alloy (filler, thickness:10 ㎛), were produced by laboratory fabrication, through casting, hot rolling, cold rolling, intermediate annealing, and final cold rolling. The effects of Si content in the core(0.04-1.05wt.%) and reduction rate of the final cold rolling(10-45%) on microstructure and brazing behavior were investigated. The results revealed that the microstructure and brazeability of the brazing sheet are governed both by Si content in the core and by the reduction rate of the final cold rolling. The excellent brazeability was obtained when the core alloy has the Si content of/cold rolled to 0.04%/10-45%, 0.41%/20-45% and 0.64%/30-45%. In these cases, a coarse grain structure was developed in the core during the brazing process, which suppressed the penetration of melting filler into the core.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.