Abstract
The composition of shielding gas was investigated for gas metal arc welding (GMAW) of the 10Ni5CrMoV steel using high Cr-Ni austenitic wire. Adding CO2 into the inert shielding gas can improve the arc stiffness and reduce the incomplete fusion of sidewall. The optimal shielding gas of 40%Ar + 58%He + 2%CO2 was applied into multi-layer multi-pass GMAW of 10Ni5CrMoV steel with austenitic wire. No welding porosity, incomplete fusion and cracks were found in the welding joint. The chemical composition of the deposited metal reached the requirement for forming austenite weld. The highest hardness of welding joint was less than 350 HV and no obvious hardening tendency occurred in the welding joint. The tensile test and impact test indicated that the multi-layer multi-pass welding joint of 10Ni5CrMoV steel using austenitic wire had excellent comprehensive mechanical properties.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.