Abstract
The effects of section size on the stress rupture lives of DD6 single crystal superalloy at 980 °C/250 MPa were investigated adopting machined thin-walled slab specimen. Stress rupture fractograph was analyzed. The results show that stress rupture lives of machined thin-walled slab specimen decline slightly with the reduction of section size at 980 °C/250 MPa, and stress rupture lives of thin-walled specimen are slightly lower compared with that of 5 mm in diameter standard cylindrically specimen, however, the stress rupture lives of thin-walled specimen are still about 200 hours. The decrease in effective loading area caused by oxidation is the main factor for the reduction of thin-walled stress rupture lives.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.