Abstract

In this study, corn straw derived biochars were prepared at different temperatures of 300, 500, 700C, respectively, and the characteristics of corn straw biochars were investigated. Additionally, the adsorption behaviors of vanadium (III, IV, V) on biochars were systematically studied by batch experiments. The absorbents were characterized by ion-exchange capacity (IEC), X-ray Diffraction, N2 adsorption-desorption, and FTIR. The yield of biochar decreases with the increase of pyrolysis temperature. The more ash content is retained, the more alkaline biochar is. The specific area of biochars increased with the rising pyrolysis temperature. With the increase of temperature, the structure became porous and the content of surface functional group elements remained low. Although the content of zinc in biochar is relatively high, the leaching toxicity of biochar does not exceed the Chinese standard. The adsorption capacity of biochars for vanadium (V) decreased under high temperature (700C). In the contrast, The adsorption capacities of biochars for vanadium (IV) and vanadium (III) improved under high temperature. The adsorption mechanisms for vanadium (V), vanadium (IV) and vanadium (III) were surface complexation, which can be proved by FTIR analysis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.