Abstract

In this study, the effects of current density and bath temperature on the hardness, thickness, and morphology of boride layer are systematically investigated. The electrochemical boride coating on steel substrates is carried out at various current densities (50–700 mA/cm2) and bath temperatures (800–1000°C) at constant electrolyte composition and electrolysis time. The FeB, Fe2B, and Fe3B phases are detected by the x-ray diffraction method. The hardness of the boride layer reaches approximately 1800 HV on the surface and gradually decreases toward the matrix. The optimum current density and electrolyte temperature for the boriding of low-alloy steel are determined as 200 mA/cm2 and 900°C, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.