Abstract
The powder of a single phase of the Al-10.7 at%Ti-0.6 at%Fe supersaturated solid solution with an average crystallite size of 11 nm has been obtained from a pure Al and Ti mixed powder by means of a high energy planetary ball mill. The mechanically alloyed (MA) powder was consolidated into cylinders 4 mm in diameter and 2.5 mm in height at temperatures of 473773 K under hydrostatic pressures of 0.1 MPa3 GPa. The consolidation at high temperatures causes the decomposition of the supersaturated solid solution obtained by MA, whereas the compacts consolidated at low temperatures retain the supersaturated solid solution and nanostructure. The upper limiting temperature where the compact can retain the supersaturated solid solution becomes higher with increasing consolidation pressure, and the application of high pressure consequently permits consolidating the MA powder at higher temperature without decomposing the supersaturated solid solution. On the other hand, the higher consolidation pressure and temperature can give higher density and hardness to the compact. Thus the application of high pressure is effective for the consolidation of MA powder with the retention of the supersaturation and nanostructure.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.