Abstract

Strontium ferrite modified 0-3 cement-based piezoelectric composites were produced with piezoelectric ceramic [0.08Pb(Li1/4Nb3/4)O•0.47PbTiO3•0.45PbZrO3], sulphoaluminate cement and strontium ferrite by compressing technique, and the effects of poling conditions on the piezoelectric and dielectric properties were investigated. In order to contrast, a unmodified 0-3 cement-based piezoelectric composite was fabricated. The results show that the higher the poling electric field, the longer the poling time and the higher the poling temperature, the composites have the higher piezoelectric strain factor d33, piezoelectric voltage factor g33, dielectric constant εr and dielectric loss tanδ, and the strontium ferrite modified composites are polarized more easily, and have better properties than the unmodified composites. In the meantime, the optimum poling conditions were obtained, and the optimum poling field E, poling time t and poling temperature T were 5 kV/mm, 20 min and 80 °C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.