Certain in vivo studies have shown that the application of adhesives directly onto the open pulp or on a thin layer of dentin causes inflammation and pulpal abscesses. This reaction is related to toxic effects of monomers from adhesives. It has been confirmed that after proper illumination the adhesives become less toxic. The aim of the study was to examine genotoxicity of non-polymerised, partly polymerised and polymerised adhesives on isolated human lymphocytes using the alkaline Comet assay. Adper Single bond2 and Adper Easy One/3M ESPE adhesive photopolymerisation was performed by Elipar Highlight 3M ESPE halogen lamp for 0, 10 and 40 sec, at final concentrations of 100, 200, 500 and 1000 ?g/mL. With both adhesives, photopolymerisation at 0 and 10 seconds showed statistically significant increase in DNA damage in comparision to the negative control (solvent). On the other hand, after 40 seconds of photopolymerisation of both adhesives in all tested concentrations, the degree of DNA damage in Comet assay had no significant difference (P>0.05, ?2 test) compared to the negative control. Therefore, only the 40 seconds of photopolymerisation prevented genotoxic effects of both adhesives in the Comet assay.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.