Abstract
The uniaxial tensile behaviors of Fe-19Cr-16Mn-2Mo-0.49N and Fe-18Cr-16Mn-2Mo-0.85N high-nitrogen and nickel-free austenitic stainless steels at two strain rates of 10−2 s−1 and 10−4 s−1 were comparatively investigated. The related deformation microstructure was characterized and fracture mechanism was analyzed. The results show that the nitrogen content and strain rate both have significant effects on the tensile properties of the tested steels. As the strain rate is the same, the tested steel containing a higher nitrogen content has higher Rm and Rp0.2. However, Rm is higher at a lower strain rate and Rp0.2 is higher at a higher strain rate in the case of the same nitrogen content. The tested steel with a lower nitrogen content (0.49 wt.%N) tensioned at a lower strain rate of 10−4 s−1 obtains the highest elongation, while the tested steel with a higher nitrogen content (0.85 wt.%N) tensioned at a higher strain rate of 10−2 s−1 has the lowest elongation. The tensile plastic deformation is mainly governed by slip and twinning, affected jointly by stacking fault energy and short-range order. Dislocation slip featured by planar slip bands and twin-like bands is the main deformation structure in the tested steel containing a higher nitrogen content (0.85 wt.%N) tensioned at a lower strain rate of 10−4 s−1, whereas twinning deformation becomes more prominent with decreasing nitrogen content and increasing strain rate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.