Abstract
The high-temperature oxidation behaviors of Co- and CoNi-base alloys with different Ni and Cr additions were investigated by isothermal oxidation in air at 900 and 1000 °C. The structure, composition, and element distribution in the three layers within the oxide scales in different alloys have been explored in detail by electron microscopy, especially with regard to the fine oxide particles in the intermediate layer. Based on the microstructure and phase constitution of the oxide scales, the synergetic effects of alloying elements on the oxidation mechanisms and resistance have been elucidated in detail with the aid of CALPHAD calculation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.