Abstract

Effects of NaN3 added in Fe—C system to synthesize nitric diamond at high pressure and high temperature are investigated. Diamond crystals with high nitrogen concentration are synthesized by the system of Fe—C and NaN3 additive at pressure 5.8 GPa and at temperatures 1750–1780K for 15 min. The synthetic diamond crystals have a cubo-octahedral or octahedral shape with yellowish green or green colour. Some disfigurements are observed on the surfaces of most diamond crystals. The composition and content of inclusions formed by iron in diamond are changed and iron nitride is detected in diamond crystals synthesized with Fe–C–NaN3 additive. As the amount of NaN3 additive increases, Fe3 C decreases and iron nitride increases with α-Fe being nearly constant. Moreover, the nitrogen concentrations in diamond crystals synthesized with 1.5wt% NaN3 additive is up to 2250 ppm in substitutional form.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.