Abstract

AbstractThe issue of moisture damage due to water intrusion in conventional road pavement is crucial due to increasing traffic load and volume, especially in the dry process. Poor workability occurs between the aggregate and binder interaction, increasing air voids in the asphalt mixture. Consequently, reduce the strength of the asphalt mixture. Hence, the additive material is one possible approach to reduce the issue. The use of treated plastic (Low-density Polyethylene) (TP) has a high potential to improve the interaction of aggregate and binder during the mixing process to against moisture damage. Further investigation on the effect of different ratios of TP content (0, 2.5, 5.0, 0.75, and 1.0% by weight of total aggregate) in asphalt mixture was studied. Mechanical performances on moisture damage of the optimum TP content in asphalt mixture were focused and evaluated with retained stability and tensile strength ratio tests. The finding revealed that 0.75% of TP content increased the resistance of moisture damage in asphalt mixtures compared to the conventional mixture.KeywordsMoisture damageAdditiveWaste polymerHot mix asphalt

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.