Abstract

The effects of Mn content and grain size on the hydrogen embrittlement resistance of face-centered cubic (FCC) CrCoFeMnNi high-entropy alloys were examined using tensile testing at an initial strain rate of 10−4 s−1. The most important finding of this study was that the combined effect of Mn removal and grain refinement provided nearly complete resistance to hydrogen embrittlement with over 800 MPa tensile strength in FCC high-entropy alloys, even after 100 MPa hydrogen gas charging.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.