ABSTRACTWe have conducted x-ray diffraction, Raman spectroscopy, and scanning electron microscopy analyses of diamond films grown by hot filament assisted chemical vapor deposition (HFCVD). We present results on the relative abundance of the (111), (220) and (400) faces in polycrystalline diamond films as functions of CH4 concentration. The intensity of the (111) peak can be varied from about 20% to 60% by adjusting CH4 in CH4/H2 mixtures. We also present results on preferred orientation in films grown under varying hydrogen treatments. We discuss correlations between the preferred orientation, FWHM of the diamond peak in the Raman spectrum, and surface morphology of the films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.