Abstract
The cast structure of M963 superalloy is greatly affected by the melt superheating treatment. Melt superheating treatment (below 1923 K) coarsens the grain structure and transforms the blocky MC carbide into Chinese-script one that mostly distributed in dendrite. However, when the melt superheating temperature reaches 2123 K, the grain structure becomes very fine equiaxed, and the morphology of MC carbide changes back to the blocky appearance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.