Abstract
We have investigated the impact of the addition to the kaolin, by mechanochemical treatment, of bonding agents such as the potassium phosphate compounds (potassium dihydrogen phosphate KH2PO4, potassium monohydrogen phosphate K2HPO4 and potassium phosphate K3PO4) on the structural, thermal and mechanical properties of the kaolin products.The fresh and sintered samples were characterized by using several techniques: X-ray diffraction (XRD), infrared spectroscopy (IR), thermal techniques (DTA/TGA and dilatometry) and the Brazilian test. The addition of the bonding agent by mechanochemical treatment minimized defects after a sintering process. This resulted in reducing the sintering temperatures.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.