In tube hydroforming, some controllable wrinkles can be used to improve the formability of tubes, so as to obtain the tubular parts with large expansion ratio and relatively uniform wall thickness. In this paper, finite element analysis and experimental research with 5052 aluminum alloy and 304 stainless steel tubes are used to investigate the effects of mechanical property parameters on wrinkling behavior of thin-walled tubes for hydroforming application. The numerical simulation results show that the effect of elastic modulus is very small and ignorable, but the initial yield stress and tangent modulus of tubes have an obvious effect on their wrinkling behavior. Tubes with higher initial yield stress and lower tangent modulus tend to possess three axisymmetric wrinkles within the lower internal pressure range. Moreover, it is found that the ratio of initial yield stress to flow stress of the tubes, σs/σf, is a significant factor to their wrinkling behavior. Three axisymmetric wrinkles could be produced on the tubes with higher σs/σf under a lower internal pressure. All of these were verified by the experimental results of 5052 aluminum alloy and 304 stainless steel tubes, whose wrinkles obtained under wrinkling internal pressure of 1.8 ps and 1.2 ps can be flattened completely in the calibration stage. These research findings are extremely meaningful to get controllable wrinkles for different kinds of tubes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.