Abstract

The role of lubrication on the consolidation behaviour of titanium powder, density increase and change in microstructure on subsequent sintering was investigated. HDH titanium powder mixed with 0-2wt% stearic acid or magnesium stearate was cold compacted. It was found that 0.3-0.6wt% of internal lubricant significantly improves the compressibility. However, more than 0.6wt% of lubricant aids the densification in the low-pressure region but limits the maximum density at high pressure. Moreover, 0.3-0.6wt% of lubricant offers a more uniform density distribution to the powder compact, while greater than 0.6wt% of lubricant leads to a segregation of lubricant in the surface region. The shape retention, ejection behaviour, de-lubrication behaviour and sintered properties were also studied in this work.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.