Abstract
In this research work, Stellite-6 was deposited on an Inconel 718 substrate via laser metal deposition (LMD) process. Lateral and vertical ultrasonic vibrations were applied during the LMD process at 150 W and 250 W to achieve improved properties. The resultant coatings were evaluated by scanning electron microscopy (SEM) equipped with an energy dispersive spectroscopy (EDS) analyzer and optical microscopy. Also, the microhardness values of two samples (without vibration and with vertical vibration) were measured. The results showed that applying ultrasonic vertical vibrations led to significant changes in the microstructure of the coatings and the coating/substrate interface i.e. a better distribution of alloying elements of the coating was achieved, the number of the secondary arms increased, and the porosity percentage decreased significantly. Moreover, the microhardness value in the sample synthesized at 150 W and under vertical vibrations were higher than that in the sample produced without vibrations.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.