Abstract
We have previously reported that the carbonate apatite (CAP) foam that has similarities in both inorganic chemical composition and morphology to cancellous bone could be prepared from α-tricalcium phosphate (α-TCP) foam by the hydrothermal treatment with Na2CO3 at 200°C for 24 hrs. However, the crystallinity of the CAP foam was much higher than that of bone. In order to prepare CAP foam similar to cancellous bone in crystallinity as well as its inorganic composition and morphology, this study attempted to prepare CAP foam at lower temperature. Hydrothermal treatment at 100°C allowed low-crystalline CAP foam whereas longer period was imposed for complete conversion of α-TCP foam into CAP foam.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.