Abstract

High temperature changes the internal microstructure of clay and consequently affects its physical and thermal properties. In this paper, the influence of firing temperature (up to 900 °C) on the thermo-physical properties of clay is analyzed through laboratory tests and the relationship between thermal conductivity and density is revealed. Furthermore, the variation of surface characteristics including clay color and cracking is reported. The results obtained indicate that the thermal conductivity and diffusivity as well as the bulk density of clay decrease rapidly as the temperature increases from room temperature to 200 °C, and then become approximately constant. From the Thermogravimetric Analysis (TG) and Differential Thermal Analysis (DTA) tests it is also shown that there are two significant stages for the clay exposed to high temperature: 25–200 °C and 400–700 °C. The evaporation of adhered water and bound water are proved to be the main reason for the first stage of clay mass loss at 25–200 °C, while the decomposition of minerals is considered as the second stage of mass loss in the temperature range of 400–700 °C. In addition, the combustion of organic matter in clay is the main reason for its darkening at 300–400 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.