Abstract
Effects of heat treatment on microstrucutures of a Re-containing single crystal superalloy have been investigated. The results showed that (γ+γ′) eutectic in as-cast alloy is practically dissolved with solution heat treatment, and the degree of segregation is distinctly decreased. The size, morphology and distribution of γ′ phase are mightily affected by the first-stage ageing treatment temperature. When the first-stage ageing treatment temperature lower than 1160°C, the shape of the γ′ phase is cubic. But the γ′ phase shape is transformed to sphericity when the temperature higher than 1180°C. The γ phase channel width is significantly increased, and the fine γ′ phase precipitated in the γ phase matrix channel.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.