Abstract

In this paper, Ti-6Al-4V alloy were successfully fabricated using a Spark Plasma Sintering (SPS), thermal deformation and heat treatment process. SPS sintering is divided into two steps: The first step is low-temperature molding at 600°C and 300 MPa, and the second step is thermal deformation at 800°C, with a deformation of 70%. The effects of solution treatment and aging process at temperatures above and below the β transformation point on the microstructure and mechanical properties of Ti-6Al-4V are investigated. The study found that the mechanical properties were better after treatment (900°C, 30 min+ water quenching +550°C, 4 h).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.