Abstract

In this study, some physical and mechanical properties of martensitic transformation in Cu–9.97 % Al–4.62 % Mn (wt%) alloy were investigated by means of X-ray diffraction (XRD), scanning electron microscopy (SEM) and compression deformation test techniques. In SEM and XRD observations of Cu–9.97 % Al–4.62 % Mn alloy, two kinds of martensitic phases: thermally and deformation effect, \({\beta_{1}^{\prime}}\) and \({\gamma_{1}^{\prime}}\) from DO3 parent phase, and the type of the produced martensite structures were noted.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.