Abstract

Grinding aids to increase grinding efficiency in cement production are materials that can produce large amounts of high-quality cement in a short time by reducing surface energy by preventing particle agglomeration and improving fluidity. In the paper, a grinding aid using glycerol-waste antifreeze(GAP) is prepared and its effect on the grinding properties of clinker is investigated in contrast to that without the grinding aid. The results are as follows: The angle of repose of the cement powder added with GAP decreases as the grinding time increases (decreases by 3.8° when the grinding time is 60 minutes), indicating that it increases the flowability of the powder. On the contrary, the residual amount of 45µm sieve is also significantly reduced (4.6% decrease) and the specific surface area increases (30.5m2/kg), which results in an increase in the grinding efficiency. In the size range of 3 to 32µm, it increases the particle content, makes the particle size distribution uniform, the 7d and 28d activity index of the powder is improved by 5% and 6%, respectively, and increases the compressive strength of the cement. In addition, it is confirmed that the performance of the TEA grinding aid and the grinding aid are similar, and are very effective in terms of economy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.