Abstract
Abstract To flake the pure aluminum powder, ball grinding and forging are used. The mechanical properties of the forged B4Cp/Al composite are tested. The results show that ball milling can flake the pure aluminum powder. The alumina layer of Al2O3 on the surface of aluminum powder are broken during the ball milling and can be dispersed in the matrix as reinforcement. The hardness of the forged aluminum with flaked Al is higher of 19.5% than that without flaked. The forging can increase ultimate tensile strength of the B4Cp/Al composite. Increasing B4C volume fraction, the average hardness of the forged B4C/Al composite with flaked Al powder gradually increases, relative density gradually decreases, ultimate tensile strength first increases and then decreases.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.