Abstract

In this paper, the finger joint of larch were taken four kind of finger length, used Larix Gmelini as materials and resorcinol resin as adhesive. This paper made a systematic study on the influence law of end pressure and finger joint strength by finger length. The research results showed that the optimal the end pressure of finger joint decreased with the increase of finger length and the finger joint strength of glued laminated timber rise with the increase of finger length. The better finger length of finger joint was 13mm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.