Bioabsorbable devices are generally susceptible to some form of degradation or alteration of material properties in response to exposure to the terminal sterilization cycle. In addition to affecting the material strength, sterilization can also increase the rate of hydrolysis, both of which can impact clinical performance. The impact of sterilization on the material/device is unpredictable and must be empirically determined. This study examined the effects of ethylene oxide treatment on the material properties of LactoSorb 82:18 poly(L-lactic acid)-poly(glycolic acid) craniofacial plates. Compared with untreated control plates, there was no effect on the initial inherent viscosity (1.3 dL/g), the glass transition temperature (58 degrees C), or on the flexural mechanical properties. Furthermore, there was no effect on the in vitro rate of hydrolysis and mechanical strength loss profile. This provides evidence that the ethylene oxide sterilization cycle is compatible with these copolymer plates and that such treatment should not affect the clinical performance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.