Abstract

Abstract The effect of metal end plates on reducing checking of pentachlorophenol-treated Douglas-fir crossarms was evaluated over 13 wet–dry cycles. Check development was variable over the first three to four cycles, and then steadily increased for both plated and nonplated ends of arms; however, both the number of checks and the maximum width of the checks were significantly lower on plated ends. The results suggest that end plating reduces the potential for deep check development in crossarms that could lead to early failure.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.