Abstract

Effects of different Sr additions (0.1%-1%Sr, mass fraction) on as-cast microstructure and tensile properties both at ambient temperature and elevated temperature of AS31 magnesium alloy were studied. The experimental results show that the addition of Sr could refine the grain size obviously and modify the eutectic Mg2Si from Chinese script shape to polyhedral shape or fine fibers shape. The addition of Sr to AS31 alloy improved the tensile strength at ambient temperature, and the ultimate strength at 150°C first decrease and then increase with the Sr addition increase from 0.1% to 1%Sr.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.