Abstract

Purpose. This study assessed the effects of dental laboratory processing variables and testing medium on porcelain adherence of representative high-palladium alloys. Material and methods. The processing variables were recasting two and three times, porcelain stripping with hydrofluoric acid and rebuilding, and changing the recommended oxidation procedures. The testing medium was air for these four groups and the nontreatment group. In the last group, the specimens were stored and tested in artificial saliva. The metal ceramic specimens were fractured with biaxial flexure in constant strain. The area fraction of adherent porcelain (%) was calculated with a standardized spectrometric technique. A gold-palladium alloy served as the control. Results. Recasting without adding new alloy negatively affected some high-palladium alloys. Porcelain stripping did not cause a decrease in adherence of the tested alloys. The alternate oxidation treatment reduced significantly the porcelain adherence of the Au-Pd and one Pd-Cu-Ga alloy. Storage and testing in artificial saliva did not significantly affect the porcelain adherence of the alloys. The Au-Pd alloy exhibited the highest porcelain adherence. (J Prosthet Dent 1998;79:514-9.)

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.