Abstract
ObjectiveThis study aimed to investigate the effect of dentin surface moisture and curing mode on microtensile bond strength (MTBS) and nanoindentation characteristics of a self-adhesive resin cement. MethodsForty-four extracted human molars were distributed into four groups according to dentin surface moisture (dry or wet) and curing mode of the resin cement (light or chemical). Clearfil SA Cement (Kuraray Noritake Dental, Japan) was used for cementation of composite cores to the pulp chamber dentin. The specimens were sectioned into beams for MTBS test at the pulpal floor. Nanoindentation hardness and creep of the cement layer were measured under 100mN load with 30s hold segment. Data were statistically analyzed using two-way ANOVA and Weibull distribution of MTBS (α=0.05). ResultsMoisture, curing mode or their interaction did not significantly affect mean MTBS values that ranged 17.6–22.6MPa (p>0.05); however, the lowest characteristic strength was found in moist chemically cured group. Hardness ranged 437–512MPa, and was not affected by the experimental factors (p>0.05). Nanoindentation creep ranged 9.3–10.9% with the chemically cured groups showing the highest values, indicating lower cross-linking and deformation resistance of their polymer network. SignificanceAdditional moisture on dentin surface did not contribute to adhesion of the anhydrous self-adhesive resin cement to dentin. Light-curing, despite attenuation through the composite core, was beneficial and improved nanoindentation creep resistance of the cement. The difference was not, however, reflected in the mean bond strength or hardness values.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.