Abstract

In the areas of remanufacturing and working conditions with requirements of wear and corrosion resistance, the WC-Co thermal spray coating has a wide applications. WC-10Co-4Cr is an excellent, has great application potential as a coating composition. In this research, the two kinds of coatings, WC-12Co and WC-10Co-4Cr, were sprayed by high velocity oxygen-flame(HVOF). The phase composition is studied by X-ray diffraction(XRD). The porosity is investigated by lase confocal scanning microscope(LCSM), and the micro-hardness is measured. The results show that, The porosity of two coatings don't differ, this maybe has relation with the parameters in the spraying process.The micro-hardness of WC-10Co-4Cr coating is higher than that of WC-12Co coating. Compared with the phase composition of WC-12Co coating, there are new phase composition Cr7C3, Cr23C6 and Cr2WO6 in the WC-10Co-4Cr coating. And the content of W2C and η phase are reduced in WC-10Co-4Cr coating. Cr had no effect on the lattice transformation of cobalt.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.