Abstract

In this study, effects of conventional shot peening, severe shot peening, re-shot peening and precised grinding were performed to AISI 1050. By two-stage operations (SSP + RSP), residual stress depth and the magnitude on the surface were quite high. While deepest compressive stress was measured in A24 + G, maximum stress was observed in A24 + N14. Grinding and re-shot peening powerfully reduced the roughness. The increase in SP intensity improved the hardness considerably, besides the most effective hardness depth was observed after A36. N7 and N14 contributed effective results in the low cycle fatigue, whereas A24, A18, A18 + N14 and A36 in high cycle fatigue.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.