The performance of biodegradable knitted and rolled 3-dimensional (3D) polylactide-based 96/4 scaffolds modified with bioactive glass (BaG) 13-93, chitosan and both was compared with regard to the viability, proliferation and chondrogenic differentiation of rabbit adipose stem cells (ASCs). Scaffold porosities were determined by micro-computed tomography (μCT). Water absorption and degradation of scaffolds were studied during 28-day hydrolysis in Tris-buffer. Viability, number and differentiation of ASCs in PLA96/4 scaffolds were examined in vitro. The dimensions of the scaffolds were maintained during hydrolysis and mass loss was detected only in the BaG13-93 containing scaffolds. ASCs adhered and proliferated on each scaffold type. Cell aggregation and expression of chondral matrix components improved in all scaffold types in chondrogenic medium. Signs of hypertrophy were detected in the modified scaffolds but not in the plain PLA96/4 scaffold. Chondrogenic differentiation was most enhanced in the presence of chitosan. These findings indicate that the plain P scaffold provided a good 3D-matrix for ASC proliferation whereas the addition of chitosan to the PLA96/4 scaffold induced chondrogenic differentiation independent of the medium. Accordingly, a PLA96/4 scaffold modified by chitosan could provide a functional and bioactive basis for tissue-engineered chondral implants.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Tissue Engineering and Regenerative Medicine
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.