Abstract

Model alloys Fe–9Cr, Fe–20Cr and Fe–20Cr–20Ni (wt.%) with Ce (0.05%, 0.1%) or Mn (1%, 2%) were exposed to Ar–20CO2 gas at 818 °C. Scales on Fe–9Cr alloys consisted of FeO and FeCr2O4, Fe–20Cr–(Ce) alloys formed only Cr2O3, and Fe–20Cr–(Mn) alloys formed Cr2O3 and MnCr2O4. All Fe–20Cr–20Ni alloys formed Fe3O4, FeCr2O4 and FeNi3. Cerium additions had little effects, but additions of 2% Mn significantly improved oxidation resistance of Fe–20Cr and Fe–20Cr–20Ni alloys. Most alloys also carburized. All alloys developed protective chromium-rich oxide scales in air. Different behavior in the two gases is attributed to faster Cr2O3 scaling rates induced by CO2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.